Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D 1525 |
Ravago Manufacturing Americas Echo® RPPC 20/10 BK Recycled Polypropylene Copolymer Polypropylene, Unreinforced, 20 MFI, 10 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT,.. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525 |
Chevron Phillips K-Resin® CK02 Styrene-Butadiene Copolymer, Blow Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: CK02 is a blow molding SBC designed to provide a softer, tougher, more flexible container while retaining the clarity and gloss of bottles produced from.. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525 |
Huntsman IROGRAN® PS 455-204 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525 |
Mitsui ADMER® NF578A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525 |
Mitsui ADMER® SE800 Elastomer Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | (50 °C/h / 50N) - B/50; ISO 306 |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | VST/B/50; ISO 306 |
Styrolution Styrolux® 684 D SBC Description: Styrolux® 684 D is a clear styrene-butadiene copolymer (SBC) used in injection molding for parts with enhanced toughness as well as in sheet and film extrusion and blow molding. Part.. |
|||
Vicat Softening Point | 58.9 °C | 138 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRF 1807 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Flow; Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525 |
Westlake EBAC® SP1802 22.5% Ethylene Butyl Acrylate Copolymer Westlake EBAC® SP1802 is a 22.5% EBA copolymer designed for blown film, tie-layer, coextrusions and blending where flexibility and strength are important. SP1802 provides excellent elasticity and l.. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525 |
DuPont Bynel® 3810 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 58.9 °C | 138 °F | ASTM D1525 |
ExxonMobil Escorene™ LD 727.22 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 727.22 is a high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Availability: North America Additive: .. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525, ISO 306 |
DuPont™ Entira® AS MK 400 Ionomer Resin Entira™ AS MK400 is an extremely hygroscopic ionomer resin that is supplied as free-flowing pellets. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525, ISO 306 |
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig.. |
|||
Vicat Softening Point | 59.0 °C @Load 1.02 kg |
138 °F @Load 2.25 lb |
ASTM D1525 |
Arkema Group LOTRYL® 15 MA 03 Copolymer Ethylene - Methyl Acrylate LOTRYL® 15 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 15 MA 03 is a polymer of .. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | 50°C/hr; 50N |
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 59.0 °C | 138 °F | ASTM D1525 |
Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to .. |