Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Orgalloy® RS 6000 Nylon 6 Alloy, Rigid Grade (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Arkema
Trade Name Orgalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orgalloy® RS 6000 Nylon 6 Alloy, Rigid Grade (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties. Non reinforced for injection molding or for the extrusion of tubes. Standard grade.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 3.3 %
3.3 %
Moisture Absorption at Equilibrium 1.3 %
1.3 %
Humidity Absorption
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 3.4 %
3.4 %
50 mm/min
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min
Tensile Creep Modulus, 1 hour 2030 MPa
294000 psi
Tensile Creep Modulus, 1000 hours 870 MPa
126000 psi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 93.0 µm/m-°C

@Temperature 20.0 °C
51.7 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 133 µm/m-°C

@Temperature 20.0 °C
73.9 µin/in-°F

@Temperature 68.0 °F
Melting Point 220 °C
428 °F
10°C/min
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Vicat Softening Point 129 °C
264 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
Dielectric Strength 38.0 kV/mm
965 kV/in
Dissipation Factor 0.025

@Frequency 1e+6 Hz
0.025

@Frequency 1e+6 Hz
0.062

@Frequency 100 Hz
0.062

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V