Polymer Property : Dielectric Strength = 965 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 38.0 kV/mm

@Temperature 23.0 °C
965 kV/in

@Temperature 73.4 °F
IEC 60243-1
DuPont Performance Polymers Rynite® 940 NC010 PET  (Unverified Data**)
Information provided by DuPont Performance Polymers
Dielectric Strength 38.0 kV/mm
965 kV/in
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance
Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical
Dielectric Strength 38.0 kV/mm
965 kV/in
IEC 60243-1
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber
PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic..
Dielectric Strength 38.0 kV/mm

@Thickness 1.00 mm
965 kV/in

@Thickness 0.0394 in
IEC 60243-1
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade
Lustran® Ultra 4000 PG is electroplating grade with high heat resistance. It is used for the production of molded plastic articles.
Dielectric Strength 38.0 kV/mm
965 kV/in
Conditioned; IEC 60243-1
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral
PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance
Dielectric Strength 38.0 kV/mm
965 kV/in
IEC 243-1
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin..
Dielectric Strength 38.0 kV/mm
965 kV/in
K20/P20; IEC 60243-1
Styrolution Luran® S KR 2863 C Colored ASA+PC
Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Dielectric Strength 38.0 kV/mm

@Thickness 1.50 mm
965 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Styrolution Novodur® 4000PG ABS
Novodur Ultra 4000PG is an injection molding grade especially suitable for electroplating, providing enhanced heat resistance.Information provided by Styrolution
Dielectric Strength 38.0 kV/mm

@Thickness 1.50 mm
965 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Styrolution Novodur® 4115 ABS
Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution
Dielectric Strength 38.0 kV/mm
965 kV/in
IEC 60243-1
Styrolution Terblend® N NM-12 ABS/PA6 (Conditioned)
Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture..
Dielectric Strength 38.0 kV/mm
965 kV/in
IEC 60243-1
Styrolution Terblend® N NMX04 ABS/PA6 (Conditioned)
Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU..
Dielectric Strength 38.0 kV/mm
965 kV/in
IEC 60243-1
Styrolution Terluran® GP-35 ABS
Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an..
Dielectric Strength 38.0 kV/mm
965 kV/in
K20/P50; IEC 60243-1
Evonik Corporation Vestamid® E55-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:They have low density.They are highly resistant to chemicals and so..
Dielectric Strength 38.0 kV/mm
965 kV/in
cond; IEC 60243-1
DSM EcoPaXX® Q-X07208 PA410-I-GF30
% Glass Reinforced, Impact Modified
Dielectric Strength 38.0 kV/mm
965 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® AG-30 PA66-GF30
Information provided by EMS Grivory
Dielectric Strength 38.0 kV/mm
965 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® AG-35 PA66-GF35
Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy ..
Dielectric Strength 38.0 kV/mm
965 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30
Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: ..
Dielectric Strength 38.0 kV/mm
965 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45
Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST..
Dielectric Strength 38.0 kV/mm
965 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33
Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti..
Dielectric Strength 38.0 kV/mm
965 kV/in
AC Rapid Rise; ASTM D149
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Dielectric Strength 38.0 kV/mm
965 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50
Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010..
Dielectric Strength 38.0 kV/mm
965 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® XE 4188 black 9992 PA612
Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v..
Dielectric Strength 38.0 kV/mm
965 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® XE 4188 nat PA612
Product description: Grilamid XE 4188 natural is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 natural are: High viscosi..
Dielectric Strength 38.0 kV/mm
965 kV/in
DAM; IEC 60243-1
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..
Dielectric Strength 38.0 kV/mm
965 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® BG-50 HM PA6-GF50
Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop..
Dielectric Strength 38.0 kV/mm
965 kV/in
IEC 60243-1
Celanese THERMX TE4004 PCT, 40% Specialty
Thermx« TE4004 NC010 is a 40% glass fiber/glass flake reinforced polycyclohexylenedimethylene terephthalate resin developed for automotive ignition systems applications. PRELIMINARY DATAInformation..
Dielectric Strength 38.0 kV/mm
965 kV/in
DAM; IEC 60243-1
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers
Dielectric Strength 38.0 kV/mm
965 kV/in
K20/P50; IEC 60243-1
Evonik Corporation Vestamid® X7099 Black 20% Glass Reinforced Nylon 612 (Conditioned)
Description: 20% glass fiber reinforced, heat-stabilizedApplications: housings, sealing and damping elements for the automotive industry, noise and vibration-dampened sliding bearings and rollersInf..
Dielectric Strength 38.0 kV/mm
965 kV/in
Evonik Corporation Vestamid® X7099 nf (dry properties) Nylon 612
ISO data as provided by the manufacturer.
Dielectric Strength 38.0 kV/mm
965 kV/in
IEC 60243-1
Celanese Thermx® TE4004 PCT, 40% Specialty  (Unverified Data**)
Thermx® TE4004 NC010 is a 40% glass fiber/glass flake reinforced polycyclohexylenedimethylene terephthalate resin developed for automotive ignition systems applications. PRELIMINARY DATA40% glass f..
Copyright © lookpolymers.com All Rights Reserved