Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Gromax
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Gromax Enterprises Corp.
Physical Properties Metric English Comments
Maximum Moisture Content 0.10
0.10
Karl Fischer
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Temperature 80.0 °C
0.0030 in/in

@Temperature 176 °F
60x60x2 mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Temperature 80.0 °C
0.0070 in/in

@Temperature 176 °F
60x60x2 mm; ISO 294-4
Melt Flow 55 g/10 min

@Load 5.00 kg,
Temperature 275 °C
55 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 92
92
[N/mm<sup>2<sup>]; ISO 7619
Tensile Strength 147 MPa
21300 psi
50 mm/min; ISO 527-1,-2
Elongation at Break 3.5 %
3.5 %
50 mm/min; ISO 527
Flexural Strength 250 MPa
36300 psi
5 mm/min; ISO 178
Flexural Modulus 7.55 GPa
1100 ksi
5 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.3 kJ/m²
4.90 ft-lb/in²
ISO 180-1A
Charpy Impact Unnotched 6.72 J/cm²

@Temperature 23.0 °C
32.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched 1.06 J/cm²

@Temperature 23.0 °C
5.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1,-3
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-1,-2
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Melt Temperature 270 - 290 °C
518 - 554 °F
ISO 294
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Drying Temperature 80.0 °C
176 °F
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour