Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets

Category Polymer , Thermoplastic , Polyurethane, TP , Silicone Polyurethane, Ether Based
Manufacturer AorTech Biomaterials
Trade Name Elast-Eon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
Tensile Strength at Break 28.0 MPa
4060 psi
Tensile Stress 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
15.0 MPa

@Strain 200 %
2180 psi

@Strain 200 %
18.0 MPa

@Strain 300 %
2610 psi

@Strain 300 %
Elongation at Break >= 400 %
>= 400 %
Modulus of Elasticity 0.115 GPa
16.7 ksi
Tear Strength 97.0 kN/m
553 pli
Copyright © lookpolymers.com All Rights Reserved