Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 97.0 kN/m | 553 pli | ISO 34B |
Huntsman AVALON® 90 AHT Thermoplastic Polyurethane AVALON® AHT TPUs are colorless, UV resistant and offer high transparency – even where parts need to be thick. With hardness levels ranging from 90 to 95 Shore A, AVALON® AHT is ideal for .. |
|||
Tear Strength | 97.0 kN/m | 553 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1685AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 97.0 kN/m | 553 pli | Die C; ASTM D624 |
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System 0.150 in. thickness. Calcium Silicate filled. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was se.. |
|||
Tear Strength | 97.0 kN/m | 553 pli | parallel; ISO 34-1 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |
|||
Tear Strength | 97.0 kN/m | 553 pli | |
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tear Strength | 97.0 kN/m | 553 pli | |
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tear Strength | 97.0 kN/m | 553 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Tear Strength | 97.0 kN/m | 553 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |