Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon MFA TFE/Perfluoromethylvinylether Copolymer

Category Polymer , Thermoplastic , Fluoropolymer , TFE/Perfluoromethylvinylether Copolymer (MFA)
Manufacturer Isoflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon MFA TFE/Perfluoromethylvinylether Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoropolymer material specifications.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ISO 12086
Water Absorption 0.025 %
0.025 %
DIN 53 495
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 60
57 - 60
DIN 53 505
Tensile Strength 28.0 - 36.0 MPa
4060 - 5220 psi
DIN 53455
Elongation at Break 250 - 360 %
250 - 360 %
DIN 53455
Tensile Modulus 0.440 - 0.480 GPa
63.8 - 69.6 ksi
DIN 53457
Coefficient of Friction, Dynamic 0.28
0.28
on steel
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C

@Temperature 20.0 - 100 °C
66.7 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 230 °C
446 °F
Continuous
Minimum Service Temperature, Air -150 °C
-238 °F
Continuous
Electrical Properties Metric English Comments
Dielectric Strength 30.0 - 35.0 kV/mm
762 - 889 kV/in
DIN 53481
Users viewing this material also viewed the following: