Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer LyondellBasell
Trade Name Hostacom™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hostacomâ„¢ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of processability, rigidity and impact and scratch and mar resistance. It was designed for automotive interior components that must have a very good impact/stiffness balance such as instrument panels or other componentry that require compliance to FMVSS201 or FMVSS208. Uses: Automotive interior partsInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 72
72
ISO 2039-2
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-1, -2
Elongation at Break 200 %
200 %
ISO 527-1, -2
Flexural Modulus 1.90 GPa
276 ksi
ISO 178
Izod Impact, Notched (ISO) 3.90 kJ/m²

@Temperature -30.0 °C
1.86 ft-lb/in²

@Temperature -22.0 °F
ISO 180
41.0 kJ/m²

@Temperature 23.0 °C
19.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
234 °F
Unannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C
135 °F
Unannealed; ISO 75A-1, -2
Shrinkage 1.0 %
1.0 %
Tool, 100x150x3.2 mm; Basell Test Method