Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.21 - 2.23 g/cc
2.21 - 2.23 g/cc
ASTM D792
Water Absorption 0.010 %
0.010 %
ASTM D570
Deformation 4.0 - 5.5 %
4.0 - 5.5 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
9.0 - 11.5 %
9.0 - 11.5 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 60
57 - 60
ASTM D2240
Ball Indentation Hardness 45.0 - 50.0 MPa
6530 - 7250 psi
ISO 2032-N132
Tensile Strength at Break >= 12.0 MPa
>= 1740 psi
ASTM D4894
Elongation at Break >= 140 %
>= 140 %
ASTM D4894
Thermal Properties Metric English Comments
Thermal Conductivity 0.340 W/m-K
2.36 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Users viewing this material also viewed the following: