Mechanical Properties Metric English Comments
Ball Indentation Hardness 45.0 MPa
6530 psi
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
Ball Indentation Hardness 45.0 MPa
6530 psi
Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
Ball Indentation Hardness 45.0 MPa
6530 psi
Murtfeldt Muralen® Polyethylene
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO.2039-2
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO.2039-2
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500
PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce..
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO.2039-2
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO 2039-1
Quadrant EPP Cesticolor™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO 2039-1
Quadrant EPP Cestilene™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO 2039-1
Quadrant EPP Cestilene™ HD 500 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO 2039-1
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data)
FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application..
Ball Indentation Hardness 45.0 MPa
6530 psi
ISO.2039-2
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500
PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce..
Ball Indentation Hardness 45.0 MPa
6530 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSS PA666
Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi..
Ball Indentation Hardness 45.0 MPa
6530 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSZ 1 PA666
Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow beha..
Ball Indentation Hardness 45.0 MPa
6530 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSZ 3 PA666
Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug..
Ball Indentation Hardness 45.0 MPa

@Time 30.0 sec
6530 psi

@Time 0.00833 hour
DIN 53 456
Hippe PE 500 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Ball Indentation Hardness 45.0 MPa
6530 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BRZ 340 H PA6
Product description: Grilon BRZ 340 H is a heat stabilized, high viscosity, impact modified PA6 extrusion grade. Grilon BRZ 340 H has the following important properties:High impact strength at low t..
Ball Indentation Hardness 45.0 - 50.0 MPa
6530 - 7250 psi
ISO 2032-N132
Adamas Adalon® 254 PTFE, 28% Glass Fiber
Information provided by Adamas, HPM