Abatron AboCast 8-19/Abocure 8-19 Epoxy  (discontinued **)

Category Polymer , Thermoset , Epoxy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8-19/Abocure 8-19 Epoxy  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.22 %
0.22 %
in 24 hours.
Viscosity Measurement 700
700
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Tensile Strength, Ultimate 39.99 MPa
5800 psi
Elongation at Break 6.5 %
6.5 %
Modulus of Elasticity 2.206 GPa
320.0 ksi
Flexural Yield Strength 57.23 MPa
8301 psi
Compressive Yield Strength 70.33 MPa
10200 psi
Izod Impact, Notched 0.246 J/cm
0.461 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 9.00e+9 ohm-cm

@Temperature 93.3 °C
9.00e+9 ohm-cm

@Temperature 200 °F
1.00e+11 ohm-cm

@Temperature 65.6 °C
1.00e+11 ohm-cm

@Temperature 150 °F
5.00e+15 ohm-cm

@Temperature 25.0 °C
5.00e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.07

@Frequency 1e+6 Hz
3.07

@Frequency 1e+6 Hz
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 2 weeks