Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.246 J/cm | 0.460 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.246 J/cm | 0.460 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers MS 110 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.246 - 1.13 J/cm | 0.460 - 2.12 ft-lb/in | Average value: 0.430 J/cm Grade Count:9 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.246 J/cm | 0.461 ft-lb/in | |
Abatron AboCast 8-17/Abocure 8-17 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 123 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |
|||
Izod Impact, Notched | 0.246 J/cm | 0.461 ft-lb/in | |
Abatron AboCast 8-19/Abocure 8-19 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.461 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Therma-Tech™ NJC-8500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 3.17 mm |
0.460 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® M-2450 Polypropylene Copolymer Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.246 J/cm | 0.460 ft-lb/in | ASTM D256 |
Global 120-PC-Natural Acrylonitrile Styrene, General Purpose Grade Description-transparent, natural, medium impact resistance, high hardness, high heat resistance, good chemical resistanceApplications-automotive, electrical parts, household goodsInformation provide.. |
|||
Izod Impact, Notched | 0.246 J/cm | 0.460 ft-lb/in | ASTM D256 |
Global 121-PC-Blue Acrylonitrile Styrene, General Purpose Grade Description-transparent, blue, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-automotive, electrical parts, household goodsInform.. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 3.20 mm |
0.460 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo GP 125BL Extrusion Molding GPPS Key features: PSP Common Uses: Sheeting, instant noodle cups.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability o.. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 3.20 mm |
0.460 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo GP 150 High Heat Resistant, High Rigidity GPPS Key features: High Heat-resistance, High Strength Common Uses: Vegetable boxes in refrigerators, humidifiers, lighting apparatus, cassette tape cases, parts of optical instruments, PS paper, etc.GPP.. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 3.20 mm |
0.460 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HI 410T Transparent HIPS Key features: Super high-gloss. Common Uses: Food container, transparent sheeting, tray, disposable cup, electronic parts packing.HIPS is a functional resin made by copolymerization of styrene monom.. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 3.20 mm |
0.460 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HI 420T Transparent HIPS Key features: Translucent Extrusion. Common Uses: Transparent toys, glass cases, various products made by injection molding needing contact-movability.HIPS is a functional resin made by copolymeriza.. |
|||
Izod Impact, Notched | 0.246 J/cm | 0.460 ft-lb/in | 0.250 inches; ASTM D256 |
TPI Porene® AS 121 PC (Blue) General Purpose SAN Porene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymers. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.460 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibiton® PB-5925 SBC Transparency, high stiffness, injection grade |
|||
Izod Impact, Notched | 0.246 J/cm | 0.460 ft-lb/in | |
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener
(discontinued **) Description:#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low v.. |
|||
Izod Impact, Notched | 0.246 J/cm @Thickness 3.20 mm |
0.460 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo GP 125 General Purpose GPPS Key features: Good-fluidity, general purpose. Common Uses: Common kitchenware, toys, general merchandise, cosmetic containers, dust covers.GPPS has excellent transparence, colorability, electric pro.. |