Category Metal , Metal Foam, Mesh, or Honeycomb , Nonferrous Metal , Aluminum Alloy , 3000 Series Aluminum Alloy
Manufacturer Hexcel
Trade Name HexWeb®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® ACG®-1 Honeycomb Aluminum Commercial Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. Five cell sizes and densities are availabe. The honeycomb is manufactured by bonding together sheets of aluminum foil which are expanded to form a cellular honeycomb confiation. The node bond adhesive is a thermosetting type, cured under heat and pressure with the honeycomb in the unexpanded or HOBE (Honeycomb Before Expansion) condition. Slices are cut from the unexpanded material to specified thickness, or cell depth, and then expanded to final confiation.The honeycomb can be supplied either expanded or in HOBE slices. Any sheet thickness between 0.125 and 20 inches can be provided. The aluminum substrate can be perforated so that all cells will be vented in a slice as thin as 0.187 inches. The perforations of the HexWeb ACG foil allow outgassing of the adhesives used to bond panel facings. Nonperforated honeycomb is also available.Applications: HexWeb ACG is a commercial grade honeycomb core offering industrial designers the advantages of an all-metal honeycomb with long service life and resistance to fungus, moisture, and temperature. Uses include industrial tooling panels , architectural panels, shelving, storage tank covers, building walls, table and countertops.
Physical Properties Metric English Comments
Density 0.0208 g/cc
0.000752 lb/in³
Nominal
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.552 MPa
80.0 psi
Bare
0.586 MPa
85.0 psi
Stabilized
Compressive Modulus 0.110 GPa
16.0 ksi
Stabilized
Shear Modulus 0.0483 GPa
7.00 ksi
Plate Shear, W Direction
0.0965 GPa
14.0 ksi
Plate Shear, L Direction
Shear Strength 0.310 MPa
45.0 psi
Plate Shear, W Direction
0.448 MPa
65.0 psi
Plate Shear, L Direction
Users viewing this material also viewed the following: