Aaron Industries AAROPRENE® G/MFN 6002 Glass and Mineral Filled Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® G/MFN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® G/MFN 6002 Glass and Mineral Filled Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 117 MPa
17000 psi
ASTM D638
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648