Arkema Group OREVAC® 9309 EVA Terpolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 9309 EVA Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as free flowing natural coloured granules. Applications include blown film extrusion, cast film coextrusion, and thermo-adhesive films.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ASTM D1505
Vinyl Acetate Content 8.0 - 9.5 %
8.0 - 9.5 %
Arkema
Melt Index of Compound 3.3 - 4.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.3 - 4.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
ASTM D2240
Tensile Strength at Break 18.0 MPa
2610 psi
ASTM D638
22.0 MPa
3190 psi
Film Property, 50 µm thickness; ASTM D882
Tensile Strength, Yield 6.00 MPa
870 psi
ASTM D638
6.00 MPa
870 psi
Film Property, 50 µm thickness; ASTM D882
Elongation at Break 500 - 700 %
500 - 700 %
Film Property, 50 µm thickness; ASTM D882
600 - 900 %
600 - 900 %
ASTM D638
Dart Drop Test 355 g
0.783 lb
ASTM D1709
Thermal Properties Metric English Comments
Melting Point 105 °C
221 °F
DSC
Vicat Softening Point 79.0 °C
174 °F
ASTM D1525
Ring & Ball Softening Point 182 °C
360 °F
Optical Properties Metric English Comments
Haze 7.6 %
7.6 %
50 micron film; ASTM D1003
Descriptive Properties Value Comments
MAH Mini 1600