Polymer Property : Gardner Impact = 16.2 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 22.0 - 36.0 J

@Temperature -30.0 - -30.0 °C
16.2 - 26.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 33.7 J Grade Count:15
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be ..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be ..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be ..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be ..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be ..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be ..
Gardner Impact 22.0 J

@Temperature 23.0 °C
16.2 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 67 mil
Axiall 2651 Rigid PVC, Molding