Material Notes:
3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates or in combination with metal or composite substrates. Superior performance is achieved on materials such as heavily plasticized PVC, EPDM, ABS, Nylon, Santoprene® and Viton®. PR1500 (formerly SB16) is a high viscosity cyanoacrylate that can be used on plastic or rubber parts that do not fit well together. It has excellent gap-filling characteristics and will not wick into unwanted areas. It has been tested and passed the requirements of Commercial Item Description A-A-3097, Type II, Class (formerly MIL-A-46050C).Information provided by 3M
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Brookfield Viscosity 1275 - 4650 cP
1275 - 4650 cP
LVF, sp 3 @ 30 rpm
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
grit-blasted steel; ISO 6922
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.333 - 1.67 min
0.00555 - 0.0278 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid