Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.333 - 1.00 min | 0.00555 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ EC2500 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Cure Time | 0.333 - 1.17 min | 0.00555 - 0.0195 hour | Time to Handling Strength |
3M Scotch-Weld™ LO1000 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Cure Time | 0.333 - 0.583 min | 0.00555 - 0.00972 hour | Time to Handling |
3M Scotch-Weld™ MG300 FLX Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.333 - 1.67 min | 0.00555 - 0.0278 hour | Time to Handling |
3M Scotch-Weld™ MG1500 PR Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.333 - 1.67 min | 0.00555 - 0.0278 hour | Time to Handling Strength |
3M Scotch-Weld™ PR1500 Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Cure Time | 0.333 - 0.833 min | 0.00555 - 0.0139 hour | Time to Handling Strength |
3M Scotch-Weld™ RT300B Rubber-Toughened Instant Adhesive 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon.. |
|||
Cure Time | 0.333 - 1.50 min | 0.00555 - 0.0250 hour | Time to Handling Strength |
3M Scotch-Weld™ RT3500B Rubber-Toughened Instant Adhesive 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon.. |