Material Notes:
Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation provided by 3M
Physical Properties Metric English Comments
Solids Content 21 - 25 %
21 - 25 %
Brookfield Viscosity 750 - 1250 cP
750 - 1250 cP
RVF #2 sp @ 20 rpm @ 27°C
Mechanical Properties Metric English Comments
Shear Strength 0.172 MPa

@Temperature 121 °C
25.0 psi

@Temperature 250 °F
Overlap, Alum/Alum
0.379 MPa

@Temperature 93.0 °C
55.0 psi

@Temperature 199 °F
Overlap, Alum/Alum
0.386 MPa

@Temperature 82.0 °C
56.0 psi

@Temperature 180 °F
Overlap, Alum/Alum
0.607 MPa

@Temperature 66.0 °C
88.0 psi

@Temperature 151 °F
Overlap, Alum/Alum
1.37 MPa

@Temperature 24.0 °C
198 psi

@Temperature 75.2 °F
Overlap, Alum/Alum
9.618 MPa

@Temperature -55.0 °C
1395 psi

@Temperature -67.0 °F
Overlap, Alum/Alum
12.49 MPa

@Temperature -34.0 °C
1811 psi

@Temperature -29.2 °F
Overlap, Alum/Alum
Peel Strength 0.701 kN/m

@Temperature 82.0 °C
4.00 pli

@Temperature 180 °F
180°, Canvas/Steel
0.877 kN/m

@Temperature 66.0 °C
5.00 pli

@Temperature 151 °F
180°, Canvas/Steel
1.75 kN/m

@Temperature 24.0 °C
10.0 pli

@Temperature 75.2 °F
180°, Canvas/Steel
2.98 kN/m

@Temperature 24.0 °C
17.0 pli

@Temperature 75.2 °F
180°, Canvas/Steel
3.07 kN/m

@Temperature -34.0 °C
17.5 pli

@Temperature -29.2 °F
180°, Canvas/Steel
3.24 kN/m

@Temperature 24.0 °C
18.5 pli

@Temperature 75.2 °F
180°, Canvas/Steel
3.68 kN/m

@Temperature 24.0 °C
21.0 pli

@Temperature 75.2 °F
180°, Canvas/Steel
4.03 kN/m

@Temperature 24.0 °C
23.0 pli

@Temperature 75.2 °F
180°, Canvas/Steel
4.73 kN/m

@Temperature 24.0 °C
27.0 pli

@Temperature 75.2 °F
180°, Canvas/Steel
1.58 kN/m

@Temperature 49.0 °C,
Time 86400 sec
9.00 pli

@Temperature 120 °F,
Time 24.0 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Jet Fuel
2.80 kN/m

@Temperature 49.0 °C,
Time 86400 sec
16.0 pli

@Temperature 120 °F,
Time 24.0 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, VMP
3.68 kN/m

@Temperature 49.0 °C,
Time 86400 sec
21.0 pli

@Temperature 120 °F,
Time 24.0 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Oil
2.10 kN/m

@Time 1.21e+6 sec
12.0 pli

@Time 336 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #11
2.28 kN/m

@Time 605000 sec
13.0 pli

@Time 168 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #11
2.63 kN/m

@Time 605000 sec
15.0 pli

@Time 168 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #12
2.63 kN/m

@Time 1.21e+6 sec
15.0 pli

@Time 336 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #12
Thermal Properties Metric English Comments
Flash Point 2.00 °C
35.6 °F
Setaflash
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Appearance Light Amber
Base Nitrile
Users viewing this material also viewed the following: