Polymer Property : Peel Strength = 18.5 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 3.24 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
18.5 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..
Peel Strength 3.24 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
18.5 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..
Peel Strength 3.24 kN/m

@Temperature 24.0 °C
18.5 pli

@Temperature 75.2 °F
180°, Canvas/Steel
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov..