Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 750 - 1000 cP | 750 - 1000 cP | resin age: 0-3 months |
Hybrid Plastics Fireban® Mark VI Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Brookfield Viscosity | 750 cP | 750 cP | |
Hybrid Plastics Fireban® Mark VII-IS Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Brookfield Viscosity | <= 750 cP | <= 750 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4201 SBR Emulsion ROVENE® 4201 is a carboxylated styrene-butadiene emulsion that has a stiff or "boardy" hand. This binder is recommended for use as a crosslink-able binder for durable nonwovens such as floor main.. |
|||
Brookfield Viscosity | <= 750 cP | <= 750 cP | #20/200 |
Mallard Creek Polymers Rovene® 4301 Styrene-Butadiene Emulsion Rovene® 4301 is a self crosslinking, carboxylated styrene-butadiene emulsion that has a very stiff hand. The binder is especially recommended for durable nonwovens such as floor maintenance pads .. |
|||
Brookfield Viscosity | <= 750 cP | <= 750 cP | #20/200 |
Mallard Creek Polymers Tylac® 4901 Self Stabilizing Latex Tylac® 4901 self stabilizing latex is a multi-functional styrene-butadiene copolymer additive for down hole cementing applications. Tylac® 4901 is designed for applications providing gas migra.. |
|||
Brookfield Viscosity | 750 - 1250 cP @Temperature 25.0 °C |
750 - 1250 cP @Temperature 77.0 °F |
25% Toluene solution; BAM 922 |
Kraton® D1111 K (SIS) Linear Block Copolymer Description: Kraton D1111 K is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
Brookfield Viscosity | 750 cP | 750 cP | 25% in toluene; ASTM D2994 |
Dynasol Solprene® 9320 Multi-branched Thermoplastic Rubber (Multi-branched SBS) Solprene® 9320 is a 68/32 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It has a non-staining FDA approved antioxidant system for food contact applications and it is essen.. |
|||
Brookfield Viscosity | 750 - 1250 cP | 750 - 1250 cP | RVF #2 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |