Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.37 MPa @Temperature 82.0 °C, Time 1.81e+6 sec |
199 psi @Temperature 180 °F, Time 504 hour |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Shear Strength | 1.37 MPa @Temperature 82.0 °C, Time 1.81e+6 sec |
199 psi @Temperature 180 °F, Time 504 hour |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Shear Strength | 1.37 MPa @Temperature 24.0 °C |
198 psi @Temperature 75.2 °F |
Overlap, Alum/Alum |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |