Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.68 kN/m @Temperature 60.0 °C, Time 605000 sec |
21.0 pli @Temperature 140 °F, Time 168 hour |
JRF, Stainless Steel; AMS-S83318 |
3M AC-250 A-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l.. |
|||
Peel Strength | 3.68 kN/m @Temperature 60.0 °C, Time 605000 sec |
21.0 pli @Temperature 140 °F, Time 168 hour |
JRF/SW, Alodine; AMS-S83318 |
3M AC-250 A-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l.. |
|||
Peel Strength | 3.68 kN/m @Temperature 23.0 °C |
21.0 pli @Temperature 73.4 °F |
Aluminum, Bell Peel |
3M Scotch-Weld™ DP405 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Peel Strength | 3.68 kN/m @Temperature 24.0 °C |
21.0 pli @Temperature 75.2 °F |
180°, Canvas/Steel |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |
|||
Peel Strength | 3.68 kN/m @Temperature 49.0 °C, Time 86400 sec |
21.0 pli @Temperature 120 °F, Time 24.0 hour |
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Oil |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |