3M Jet-melt™ 3731 Polyolefin Bonding Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Jet-melt™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Jet-melt™ 3731 Polyolefin Bonding Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provided by 3M
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
Brookfield Viscosity 12000 cP
12000 cP
#276 sp @ 10 rpm
Mechanical Properties Metric English Comments
Shear Strength 1.77 MPa
257 psi
Overlap, Polystyrene (High Impact)
2.69 MPa
390 psi
Overlap, Cold Rolled Steel
2.90 MPa
420 psi
Overlap, HDPE
2.96 MPa
430 psi
Overlap, PVC (Rigid)
2.96 MPa
430 psi
Overlap, Polycarbonate
3.10 MPa
450 psi
Overlap, ABS
3.28 MPa
475 psi
Overlap, Nylon 66
3.38 MPa
490 psi
Overlap, Douglas Fir
3.79 MPa
550 psi
Overlap, Polypropylene
Impact Test 9.04 J
6.67 ft-lb
Peel Strength 2.63 kN/m
15.0 pli
180° Canvas to Polystyrene (High Impact)
2.63 kN/m
15.0 pli
180° Canvas to Cold Rolled Steel
3.16 kN/m
18.0 pli
180° Canvas to PVC (Rigid)
3.33 kN/m
19.0 pli
180° Canvas to Nylon 66
3.86 kN/m
22.0 pli
180° Canvas to Polypropylene
3.86 kN/m
22.0 pli
180° Canvas to Polycarbonate
4.03 kN/m
23.0 pli
180° Canvas to HDPE
4.03 kN/m
23.0 pli
180° Canvas to ABS
Thermal Properties Metric English Comments
Flash Point 273 °C
523 °F
COC
Ring & Ball Softening Point 157 °C
315 °F
ASTM E28-607