Mechanical Properties Metric English Comments
Impact Test 9.04 J
6.67 ft-lb
Direct and Reverse; ASTM D2794-84
Lord Adhesives Aeroglaze® Z3480 High Solids Aromatic Polyurethane Coating
Aeroglaze® Z3480 coating is designed for use on properly prepared and primed metal surfaces, in regions requiring a VOC below 335.8 g/l (2.8 lbs/gallon).All information provided by Lord.
Impact Test 9.04 J
6.67 ft-lb
direct; ASTM D2794
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound
An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b..
Impact Test 9.04 J
6.67 ft-lb
Reverse; ASTM D2794
Chesterton ARC MX1 Vertical Build Extreme Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”)..
Impact Test 9.04 J
6.67 ft-lb
direct; ASTM D2794
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating
Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres..
Impact Test >= 9.04 J
>= 6.67 ft-lb
Intrusion; ASTM D2794
Chesterton 752 Cold Galvanizing Compound
Description: Chesterton® 752 Cold Galvanizing Compound functions both as a zinc rich primer or final coating for ferrous metals and their welds exposed to atmospheric or corrosive conditions. The p..
Impact Test 9.04 J
6.67 ft-lb
Direct; ASTM D2794
Chesterton ARC MXC Castable Extreme Wear Compound
Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro..
Impact Test 9.04 J
6.67 ft-lb
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive
3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide..
Impact Test 9.04 J
6.67 ft-lb
ASTM A775
3M Scotchkote™ 412 Fusion Bonded Epoxy Coating
3M Scotchkote Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to preheated steel..
Impact Test 9.04 J
6.67 ft-lb
ASTM A775
3M Scotchkote™ 412 Spray Grade Fusion Bonded Epoxy Coating
3M Scotchkote Spray Grade Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to pre..
Impact Test 9.04 J
6.67 ft-lb
Blue River Coatings Wood Primer
BLUE RIVER COATINGGS WOOD PRIMER is a high quality, single component primer, not requiring any catalyzing agent. WOOD PRIMER offers good coverage, excellent durability, and ease of application, as w..