Polymer Property : Shear Strength = 430 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 2.96 MPa
430 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 3/8-5052-.004 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 2.96 MPa
430 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 5/32-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 2.96 MPa
430 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 2.96 MPa
430 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 5/32-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 2.96 MPa
430 psi
Overlap, PVC (Rigid)
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive
3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide..
Shear Strength 2.96 MPa
430 psi
Overlap, Polycarbonate
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive
3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide..
Shear Strength 2.96 MPa

@Temperature 82.0 °C
430 psi

@Temperature 180 °F
Aluminum, Overlap; ASTM D1002
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
Shear Strength 2.96 MPa
430 psi
On Douglas Fir
3M Scotch-Weld™ 3747 Hot Melt Adhesive
General purpose for wide variety of plastics, wood and lightweight metalsInformation provided by 3M