Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 2.69 MPa | >= 390 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR III 1/4-5052-.004 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 2.69 MPa | >= 390 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRP - 3/16 - 5.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 2.69 MPa | 390 psi | Plate Shear, L Direction, typ, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Shear Strength | >= 2.69 MPa | >= 390 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 2.69 MPa | 390 psi | Overlap, Cold Rolled Steel |
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive 3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide.. |
|||
Shear Strength | 2.69 MPa | 390 psi | Overlap, PVC/PVC, Rigid |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 2.69 MPa | 390 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polycarbonate |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 2.69 MPa | 390 psi | On Douglas Fir |
3M Scotch-Weld™ 3764 Hot Melt Adhesive Bonds variety of plastics including polycarbonate, polyethylene, and polypropylene and Flexible at low temperaturesInformation provided by 3M |