Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.77 MPa | 257 psi | Overlap, Polystyrene (High Impact) |
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive 3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide.. |