Mechanical Properties Metric English Comments
Shear Strength >= 3.10 MPa
>= 450 psi
Lap
Parker Chomerics CHO-BOND 1029 Conductive Adhesive
CHO-BOND® 1029 is a highly conductive silicone adhesive, intended for bonding Chomerics’ conductive silicone EMI gaskets to electrically conductive substrates. It is a two-component, siliver-plate..
Shear Strength 3.10 MPa
450 psi
Plate Shear, W Direction, typ, preliminary value obtained from limited testing
Hexcel® HexWeb® CFC™-20-1/8-11.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..
Shear Strength >= 3.10 MPa
>= 450 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..
Shear Strength 3.10 MPa
450 psi
Plate Shear, L Direction
Hexcel® HexWeb® HRH-78 - 3/16 - 6.0 Commercial Grade Nomex Honeycomb/Phenolic Resin
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after..
Shear Strength >= 3.10 MPa
>= 450 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRP - 1/4 - 6.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 3.10 MPa
450 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP - 3/8 - 8.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 3.10 MPa
450 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 3.10 MPa
450 psi
Overlap, ABS
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive
3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide..
Shear Strength 3.10 MPa
450 psi
Overlap, PVC
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb..
Shear Strength 3.10 MPa

@Temperature 66.0 °C
450 psi

@Temperature 151 °F
Overlap
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b..
Shear Strength 3.10 MPa

@Temperature 82.0 °C,
Time 900 sec
450 psi

@Temperature 180 °F,
Time 0.250 hour
Aluminum Overlap
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 3.10 MPa
450 psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polystyrene
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 3.10 MPa
450 psi
Overlap, Gasoline for 14 days, Cohesive Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 3.10 MPa

@Temperature 32.0 °C
450 psi

@Temperature 89.6 °F
Overlap, Aluminum, 90% RH, Adhesive Failure
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 3.10 MPa
450 psi
Overlap, Pine, Substrate/Cohesive Failure
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 3.10 MPa
450 psi
Overlap, MDF, Cohesive Failure
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 3.10 MPa

@Temperature 32.0 °C
450 psi

@Temperature 89.6 °F
Overlap, Aluminum, 90% RH, Adhesive Failure
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 3.10 MPa
450 psi
Overlap, Isopropyl Alcohol Wipe surface prep, ABS PVC
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 3.10 MPa
450 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polyacrylic
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 3.10 MPa
450 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polystyrene
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Copyright © lookpolymers.com All Rights Reserved