Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 12000 cP | 12000 cP | #276 sp @ 10 rpm |
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive 3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide.. |
|||
Brookfield Viscosity | 12000 cP @Temperature 191 °C |
12000 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 3731 Hot Melt Adhesive High heat resistance and Bonds plastics including polyethylene, polypropyleneInformation provided by 3M |
|||
Brookfield Viscosity | 12000 - 16000 cP | 12000 - 16000 cP | RVT #3 @ 2.5 rpm |
3M Scotch-Weld™ HP45 Pipe Sealant Anaerobic Adhesives 3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. H.. |