Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tygon® Ultra Chemical Resistant Tubing offers a combination of chemical resistance, clarity and flexibility. Tygon® 2375 replaces 2075.Tygon® Ultra Chemical Resistant Tubing is virtually unaffected by acids, bases, ketones, salts and alcohols, fitting the requirements of many applications from battery acid filling to hazardous material handling. It's entirely plasticizer-free, eliminating fluid contamination and the premature embrittlement and cracking common with many flexible tubings. Its exceptionally smooth inner surface inhibits particulate buildup and reduces the potential for contamination. Applications Battery acid filling Clean and degreaser transfer systems Fine and specialty chemical production Hazardous materials handling Ink and printing fluid dispensing Paint and solvent production Power generation sampling and drain lines X-ray processing Features and Benefits Resistant to highly aggressive chemicals Plasticizer-free -- minimizes risk of fluid contamination Exceptionally smooth inner surface inhibits particulate buildup Low sorption maintains fluid integrity Meets USP Class VI criteria Regulatory Information: This product complies with FDA and NSF 51 criteria. Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM plaques or molded ASTM durometer buttons.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Water Absorption <= 0.010 %

@Temperature 22.8 °C,
Time 86400 sec
<= 0.010 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 75

@Time 15.0 sec
75

@Time 0.00417 hour
ASTM D2240
Tensile Strength 13.1 MPa
1900 psi
ASTM D412
Elongation at Break 850 %
850 %
ASTM D412
100% Modulus 0.00293 GPa
0.425 ksi
ASTM D412
Tear Strength 42.1 kN/m
240 pli
ASTM D1004
Compression Set 100 %

@Temperature 70.0 °C,
Time 79200 sec
100 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Tensile Set 300 %

@Strain 75.0 %
300 %

@Strain 75.0 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 54.4 °C
130 °F
Minimum Service Temperature, Air -75.0 °C
-103 °F
temperature limit for flexibility
Brittleness Temperature -75.0 °C
-103 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear, but value not quantified
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
USP Class VI Yes
Yes
Descriptive Properties Value Comments
Color Clear