Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.5 MPa | 2100 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8001 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible K85 Natural & Black Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | Data derived from type IV specimen, 75 mil plaque @ 20" min.; ASTM D638 |
LyondellBasell Petrothene® NA960000 Low Density Polyethylene ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PE3-0202ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PE3-0205ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compo.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D412 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black Information provided by ITW Devcon |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Blow Molding) ApplicationsPETROTHENE NA 940-000 is a low density homopolymer resin intended for use in blow molding applications. Excellent toughness, good clarity and processability make NA 940-000 an ideal cho.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
Teknor Apex APEX® 157V-4 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Low to no Migration; Oil Resistant; Good UV Resistance; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing; Wire and Cable Applications; Au.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
Teknor Apex APEX® 3611-65 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
Teknor Apex APEX® 84217 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
Teknor Apex Fireguard® 910L16-C1A-NL1 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Ar.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1473 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1479 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1479F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1479-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1500 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
Teknor Apex APEX® 3801-80 Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7100-40D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | |
Daikin DAI-EL G-755 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Extrusion of hose and tubing, etc.Information provided by Daikin Indus.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | |
3M EPS-300 Heat Shrink Tubing 3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | |
3M VFP-876 Tubing 3M VFP-876 is the most flexible of the heat-shrinkable, polyolefin tubings. Rated at 135°C. VFP-876 Tubing has been engineered to offer a low shrink temperature of 100°C. This allows the tubing to.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
ExxonMobil Paxon™ AM55-003 Blow Molding Resin
(discontinued **) AM55-003 is a blow molding grade high density polyethylene copolymer containing an excellent antistat additive. It provides a good combination of stiffness and stress crack resistance. AM55-003 co.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | ASTM D638 |
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
(discontinued **) AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance.Information provided by Exx.. |
|||
Tensile Strength at Break | 14.5 MPa | 2100 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WC9000L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |