Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 300 °C | 572 °F | |
Premix Thermoplastics PREBLACK PE 700-30 PREBLACK PE 700-30 is a polyethylene based black masterbatch. PREBLACK PE 700-30 has been developed for the coloring of PE-LD and PE-HD products when maximum UV-resistance and pureness is being requ.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | Deflection Temperature, Load not specified; ASTM D648 |
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | Short Term |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | short term |
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | DIN 53772 |
Karina 1000/00856-IE MBPEB White Mineral concentrated, recommended for polyolefinic material. Non-toxic, adequate for using with food (Kind I, II, IIIA, IIIB, IV, V, and VI) according to Resolution 105 Anvisa. Usage from 3 to 20%.I.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
Lucite International Colacryl ® P2608 Specialty Polystyrene Resin Cross-linked polystyrene resins have much higher thermal stability than conventional thermoplastic acrylic resin. Colacryl® P2608 is stable up to around 300°C.Suggested Uses:-Glass interleavan.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | Heat Resistance; DIN 53772 |
Karina E 1000/6000-IE MBPEB White Color Concentrate Pigment preparation containing 60% TIO2, dispersed in polyethylene suitable for coloring polyolefins in both extrusion and injection molding process.Information provided by Karina Indústria e Com.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | Short Periods |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
Ensinger TECASINT 1101 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | Intermittent |
Epoxy Technology EPO-TEK® 330 Low Viscosity, Optical Epoxy Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications.Advan.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | Intermittent |
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | Intermittent |
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy Material Description: A single component, UV curable epoxy, designed for adhesive, sealing, and encapsulating applications found in semiconductor, electro-optics, fiber optics, medical, and scientif.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | Continuous |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
BASF Heligoen® Blue L 6990 F Color Additive Description: Highly transparent Phthalocyanine blue pigment with neutral flopChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Ac.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
BASF Heligoen® Blue L 9630 Color Additive Description: Transparent a-phthalocyanine blue –especially for effect shade Chemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Ac.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
BASF Heligoen® Green K 8683 Color Additive Chemical Structure: Cu-phthalocyanine chlorinate Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, CA/CAB, and UPRecommendations for food applications: BgV.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
Alliance S-30A Samarium Cobalt Magnetic Material |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
Alloy Wire International RW 70 Hot Cutting Wire - High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
BACT DLC Diamond-Like Coating DLC (a-C:H). This coating provides the highest hardness and abrasion resistance of the BACT products. Typical applications include high wear environments involving seals, molds, metal forming, and.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
BASF Sicopal® Yellow K 1160 FG Color Additive Chemical Structure: Bismut-vanadium oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA and PARecommendations for food applications: BgVV, FrancePhysical form.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | for short periods |
3M VFP-876 Tubing 3M VFP-876 is the most flexible of the heat-shrinkable, polyolefin tubings. Rated at 135°C. VFP-876 Tubing has been engineered to offer a low shrink temperature of 100°C. This allows the tubing to.. |
|||
Maximum Service Temperature, Air | 300 °C | 572 °F | |
Dow Corning 3120 RTV SILICONE RUBBER Two-part, red, condensation cure, moderate flow, high temperature performance, UL HB, cure speed varied by catalyst type and mix ratio.Information provided by Dow Corning |