Material Notes:
3M Aerospace Sealant AC-360 A-2 is a fast cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealant. 3M AC-360 A-2 Sealants maintain flexibility and bond strength on most metal substrates such as aluminum, titanium, steel, stainless steel, and many coatings under extremes of temperature, weathering and stress. The mixed compound is a pourable liquid easily applied by brush or roller. It has excellent tooling properties.Information provided by 3M
Physical Properties Metric English Comments
Density <= 1.40 g/cc
<= 0.0506 lb/in³
cured 14 days @ 50% RH
Volatiles 12 %
12 %
Brookfield Viscosity 10000 - 35000 cP
10000 - 35000 cP
Base, RVF #6 sp @ 10 rpm
Mechanical Properties Metric English Comments
Hardness, Shore A 48 - 53
48 - 53
cured 14 days @ 50% RH
Tensile Strength at Break 1.52 MPa
220 psi
Standard Cure
2.08 MPa
302 psi
7 days JRF
Elongation at Break 386 %
386 %
Standard Cure
506 %
506 %
7 days JRF
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
cured 14 days @ 50% RH
182 °C
360 °F
Short term, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
cured 14 days @ 50% RH
Processing Properties Metric English Comments
Cure Time 420 - 540 min
7.00 - 9.00 hour
480 min
8.00 hour
Tack-Free Time
Shelf Life 2.00 - 6.00 Month

@Temperature <=26.7 °C
2.00 - 6.00 Month

@Temperature <=80.1 °F
Descriptive Properties Value Comments
Appearance Dark Brown
Accelerator
Dark Gray
Off White
Base