Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 420 min | 7.00 hour | 2 hrs @ 25°C + 5 hrs @ 55°C |
Tra-Con Tra-Cast 3011 Semi-Flexible Clear Epoxy Casting Compound TRA-CAST 3011 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life.. |
|||
Cure Time | 420 min | 7.00 hour | 2 hrs @ 25°C + 5 hrs @ 55°C |
Tra-Con Tra-Cast 3012 Clear Epoxy Casting Compound TRA-CAST 3012 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties good clarity, long pot life,.. |
|||
Cure Time | 420 min | 7.00 hour | 2 hrs @ 25°C + 5 hrs @ 55°C |
Tra-Con Tra-Cast FS255 Flexible Clear Epoxy Casting Compound TRA-CAST FS-255 is a clear, low viscosity, epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties -- good clarity, long pot.. |
|||
Cure Time | 420 min | 7.00 hour | |
3M AC-251 Black Class B-1 Aerospace Sealant 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai.. |
|||
Cure Time | 420 - 480 min | 7.00 - 8.00 hour | Tack-Free Time |
3M AC-350 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Cure Time | 420 - 480 min | 7.00 - 8.00 hour | |
3M AC-350 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Cure Time | 420 - 540 min | 7.00 - 9.00 hour | |
3M AC-360 A-2 Aerospace Sealant 3M Aerospace Sealant AC-360 A-2 is a fast cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealant. 3M AC-360 A-2 Sealants maintain fle.. |
|||
Cure Time | 420 - 480 min | 7.00 - 8.00 hour | Tack-Free Time |
3M AC-770 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio.. |
|||
Cure Time | 420 min | 7.00 hour | Full |
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |
|||
Cure Time | 420 - 600 min | 7.00 - 10.0 hour | 1-4 hrs Air Set; 2 hrs at 200°F; 2 hrs at 500°F; 2 hrs at 700°F |
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Cure Time | 420 - 480 min | 7.00 - 8.00 hour | Tack-Free Time |
3M AC-370 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Cure Time | 420 min | 7.00 hour | Full |
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |
|||
Cure Time | 420 min | 7.00 hour | Tack-Free Time |
3M AC-236 Class A-1/2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class A are brushable, two-component, liquid polysulfide polymer sealant providing excellent fuel tank and fuselage seals. They have outstanding resistance to aviation ga.. |