Mechanical Properties Metric English Comments
Tensile Strength at Break 2.08 MPa
302 psi
7 days JRF
3M AC-360 A-2 Aerospace Sealant
3M Aerospace Sealant AC-360 A-2 is a fast cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealant. 3M AC-360 A-2 Sealants maintain fle..