Polymer Property : Tensile Strength at Break = 220 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 1.52 MPa
>= 220 psi
ASTM D412
Parker Chomerics CHO-SEAL 1260 Conductive Elastomer
Conductive Elastomer. CHO-SEAL 1260 elastomer is a silver-filled-silicone intended for mounting silicon wafers during processes such as ion milling. It provides high levels of electrical and thermal..
Tensile Strength at Break 1.52 MPa

@Temperature 23.0 °C
220 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G6713C Thermoplastic Elastomer (TPE)
Dynaflex™ G6713C is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV Sta..
Tensile Strength at Break 1.52 MPa
220 psi
(20 in/min), Molded Properties; ASTM D638
ExxonMobil Escorene™ MV 02528EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 02528EH2 is a copolymer of ethylene and vinyl acetate.Availability: Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent: Yes A..
Tensile Strength at Break 1.52 MPa
220 psi
Standard Cure
3M AC-360 A-2 Aerospace Sealant
3M Aerospace Sealant AC-360 A-2 is a fast cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealant. 3M AC-360 A-2 Sealants maintain fle..
Tensile Strength at Break 1.52 MPa
220 psi
50% RH
3M PN8029 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..