3M 7901 Screen Printable Sheet Vinyl Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7901 Screen Printable Sheet Vinyl Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utilizes 3M™ Adhesive 500, a high stability acrylic adhesive, which provides excellent adhesive to a variety of surfaces including stainless steel, polycarbonate and polypropylene. This adhesive features one-piece removal up to one year after application and is designed for indoor/outdoor use.Information provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Adhesive
86.4 microns
3.40 mil
Facestock
170 microns
6.70 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.09861 kN/m
0.5625 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.110 kN/m
0.625 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.110 kN/m
0.625 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1205 kN/m
0.6875 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.131 kN/m
0.750 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.131 kN/m
0.750 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.1424 kN/m
0.8125 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1424 kN/m
0.8125 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.153 kN/m
0.875 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.153 kN/m
0.875 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.1643 kN/m
0.9375 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.18626 kN/m
1.0625 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.18626 kN/m
1.0625 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.18626 kN/m
1.0625 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.1972 kN/m
1.125 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.1972 kN/m
1.125 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.20817 kN/m
1.1875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.23008 kN/m
1.3125 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.25199 kN/m
1.4375 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.263 kN/m
1.50 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.263 kN/m
1.50 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.2849 kN/m
1.625 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.2849 kN/m
1.625 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.29582 kN/m
1.6875 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.31773 kN/m
1.8125 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.33964 kN/m
1.9375 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.351 kN/m
2.00 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.40538 kN/m
2.3125 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.4163 kN/m
2.375 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.42729 kN/m
2.4375 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.44921 kN/m
2.5625 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.5040 kN/m
2.875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.51494 kN/m
2.9375 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.570 kN/m
3.25 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.570 kN/m
3.25 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.6355 kN/m
3.625 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.64642 kN/m
3.6875 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.745 kN/m
4.25 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.789 kN/m
4.50 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.8108 kN/m
4.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
5.00 °C
41.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 500
Liner 90# Polyctd.