Mechanical Properties Metric English Comments
Peel Strength 0.20817 kN/m
1.1875 pli
LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
3M 7000 Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.20817 kN/m
1.1875 pli
LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
3M 7000FL Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.20817 kN/m
1.1875 pli
LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
3M 7000FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.20817 kN/m
1.1875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7600 Removable Vinyl Label Material
3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent..
Peel Strength 0.20817 kN/m
1.1875 pli
Polypropylene, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
3M 7735FL Acrylate Overlaminating Film
3M™ Acrylate Overlaminating Film 7735FL utilizes an outdoor durable acrylate film facestock with exceptional UV resistance, combined with 3M™ Adhesive 400 and a film liner. This product offers exc..
Peel Strength 0.20817 kN/m
1.1875 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7735FL Acrylate Overlaminating Film
3M™ Acrylate Overlaminating Film 7735FL utilizes an outdoor durable acrylate film facestock with exceptional UV resistance, combined with 3M™ Adhesive 400 and a film liner. This product offers exc..
Peel Strength 0.20817 kN/m
1.1875 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7744FL Polyester Overlaminating Film
3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l..
Peel Strength 0.20817 kN/m
1.1875 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7745FL Polyester Overlaminating Film
3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r..
Peel Strength 0.20817 kN/m
1.1875 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7779 Polypropylene Label Material
3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating..
Peel Strength 0.20817 kN/m
1.1875 pli
Finely Textured Powder Coating, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7779 Polypropylene Label Material
3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating..
Peel Strength 0.20817 kN/m
1.1875 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7850TL Laser Toner Printable Polyester Label Material
3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for..
Peel Strength 0.20817 kN/m
1.1875 pli
Adhesion to Steel; ASTM D3330
3M 5700 Safety Stripe Tape
3M™ Safety Stripe Tapes are durable vinyl tapes used to identify and mark traffic areas and physical hazards.Information provided by 3M
Peel Strength 0.20817 kN/m
1.1875 pli
Adhesion to Steel; ASTM D3330
3M 5702 Safety Stripe Tape
3M™ Safety Stripe Tapes are durable vinyl tapes used to identify and mark traffic areas and physical hazards.Information provided by 3M
Peel Strength 0.20817 kN/m
1.1875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7901 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili..
Peel Strength 0.20817 kN/m
1.1875 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7920 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive ..
Peel Strength 0.20817 kN/m
1.1875 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7744 Polyester Overlaminating Film
3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l..
Peel Strength 0.20817 kN/m
1.1875 pli
HDPE, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
3M 7776 Polypropylene Label Material
3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh..
Peel Strength 0.20817 kN/m
1.1875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
3M 7776 Polypropylene Label Material
3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh..
Peel Strength 0.20817 kN/m
1.1875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7884 White Vinyl Label Material
Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and..