3M 7731FL Polyester Overlaminating Film

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7731FL Polyester Overlaminating Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature performance and long term aging for resistance to yellowing in outdoor applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 20.3 microns
0.800 mil
Adhesive
38.1 microns
1.50 mil
Liner
50.8 microns
2.00 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.49303 kN/m
2.8125 pli
Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.526 kN/m
3.00 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.55877 kN/m
3.1875 pli
Polyester, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.657 kN/m
3.75 pli
Polyester, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
-12.0 °C
10.4 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type #400 Acrylic
Liner Clear Polyester Liner