Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | |
ConocoPhillips Tacna® HD Grease NLGI Grade 2 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | |
Dow Corning MOLYKOTE® G-0052 FG WHITE EP BEARING GREASE Aluminum complex-thickened mineral oil food grade greaseInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | |
ChevronTexaco NLGI 1 Moly MAX Grease EP FeaturesChevron Moly MAX Greases EP are high performance greases.They are formulated with extreme pressure additives and 5% molybdenum disulfide (moly). They are dark gray/black in color and smooth .. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | |
ChevronTexaco Thread Sealing Compound FeaturesChevron Thread Sealing Compound is a time-tested aluminum complex grease designed especially for casing and tubing connections in high-pressure oil well service, or wherever unusually severe.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | |
ChevronTexaco Tool Joint Compound FeaturesChevron Tool Joint Compound is an aluminum complex grease designed principally for the lubrication of drill collars, tool joints and pipe threads.It contains copper flake and graphite, forti.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | JIS-K-6723 |
Denka VINYKON W4050 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | See Note 1. |
ChevronTexaco Crater® A Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Gehman torsion test, T10 |
Daikin DAI-EL G-551 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7250 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7732FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7737FL Velvet Textured Polycarbonate Overlaminating Film 3M™ Velvet Textured Polycarbonate Overlaminating Films 7737FL and 7738FL utilize velvet textured polycarbonate film to achieve a decorative velvet appearance. 3M™ Adhesive 400 offers excellent low.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7741 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7743FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | |
3M 9740 Double Coated Tape 3M™ Double Coated Tape 9740 is a 3.5 mil double coated tape utilizing a 0.5 mil (12 microns) polyester film coated on both sides with 1.5 mils (38 microns) of a high shear acrylic adhesive system. .. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M Scotchrap™ 51 Tape 3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7120 Performance Paper Label Material 3M™ Label Materials 7120 and 7122 latex impregnated paper with 3M™ 400 and 320 adhesives offer good conformability to curved surfaces and resistance to staining and moisture. Label Material 7120 h.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7225 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7237 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1400, which is a high performance tackified acry.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7242 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1400, which is a high performance tackified acry.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7244 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7710 Acetate Identification Label Material 3M™ Label Material 7710 gloss clear acetate with 3M™ 400 high tack acrylic adhesive offers consistent, high quality appearance and excellent UV resistance. The transparent film easily die-cuts whi.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7731FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7730FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7733FLW Overlaminating Film 3M™ Overlaminating Film 7733FLW utilizes a clear polyester film that is recommended for optimum durability and superior outdoor UV exposure and print fade protection. 3M™ Adhesive 400 offers excel.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Application |
3M 7742 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Minimum Service Temperature, Air | -12.0 °C | 10.4 °F | Temperature retraction (TR-10) |
Dow Advanta® 3302 Specialty Elastomer
(discontinued **) Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000.. |