Material Notes:
Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility, UL V-0.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 2.36 g/cc

@Temperature 25.0 °C
2.36 g/cc

@Temperature 77.0 °F
Viscosity 14000 cP
14000 cP
dynamic
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 57
57
Thermal Properties Metric English Comments
Thermal Conductivity 1.26 W/m-K
8.74 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+15 ohm-cm
7.00e+15 ohm-cm
Dielectric Constant 6.0

@Frequency 1.00e+6 Hz
6.0

@Frequency 1.00e+6 Hz
Dielectric Strength 5.00 kV/mm
127 kV/in
Processing Properties Metric English Comments
Cure Time 45.0 min

@Temperature 125 °C
0.750 hour

@Temperature 257 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color grey
Hydrophobic yes
Self Leveling yes
Water Resistant yes
Working Time (min) 300