Haysite 20000 Polyester BMC, 15% Glass Reinforced

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Haysite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite 20000 Polyester BMC, 15% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 20000 series bulk molding compound is an electrical grade that can be compression, transfer, or injection molded. Offering good arc/track properties and mechanical strength, this grade is also recognized by UL with a 94V-0 flame rating at .060" wall thickness. Haysite 20000 BMC has a slightly higher shrinkage rate than other Haysite UL recognized BMC's.
Physical Properties Metric English Comments
Density 1.95 g/cc
0.0704 lb/in³
ASTM D572
Water Absorption 0.10 %
0.10 %
ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
Flexural Strength 103 MPa
14900 psi
Compressive Strength 90.0 MPa
13100 psi
Izod Impact, Notched 2.10 J/cm
3.93 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Flammability, UL94 V-0
V-0
File No.E-27875
Electrical Properties Metric English Comments
Dielectric Constant 5.5

@Frequency 60 Hz
5.5

@Frequency 60 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
Perpendicular (ASTM D149), Short Time
Dissipation Factor 0.029

@Frequency 60 Hz
0.029

@Frequency 60 Hz
ASTM D150
Arc Resistance 190 sec
190 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: