Polycasa PETG

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Polycasa
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polycasa PETG.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits of QUINN PETG are its very good chemical resistance and very high impact properties. QUINN PETG meets all current food contact legislation and can be used in contact with unwrapped food. QUINN PETG also combines the following excellent properties: easy to vacuum form, needs no predrying, exceptional low temperature performance, low water absorption, ease to recycle, and very high impact propertiesBus shelters Poster glazing Machine guards Medical appliance packaging Displays & signs for external use Refrigerators and cold storeroom equipment Bicycle safety helmets Food containers Lenticular lenses Graphic Arts Lighting controllers for hazardous areasQuinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D1595
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength at Break 50.0 MPa
7250 psi
DIN 53455
Elongation at Break 54 %
54 %
DIN 53466
Tensile Modulus 2.20 GPa
319 ksi
DIN 53455
Flexural Strength 70.0 MPa
10200 psi
DIN 53452
Flexural Modulus 2.075 GPa
301.0 ksi
DIN 53452
Izod Impact, Notched (ISO) 11.5 kJ/m²
5.47 ft-lb/in²
ISO 180
Charpy Impact Unnotched NB
NB
DIN 53453
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C

@Temperature 20.0 °C
37.8 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
ASTM D2766
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 70.0 °C
158 °F
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
DIN 53461
Vicat Softening Point 82.0 °C
180 °F
DIN 53460
Decomposition Temperature >= 280 °C
>= 536 °F
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
DIN 53491
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Transmission, Visible 88 %
88 %
DIN 5036-3
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+16 ohm
>= 1.00e+16 ohm
ASTM D257
Dielectric Constant 2.6

@Frequency 100 Hz
2.6

@Frequency 100 Hz
Dielectric Strength 16.0 kV/mm
406 kV/in
D149
Dissipation Factor 0.010

@Frequency 50 Hz
0.010

@Frequency 50 Hz
IEC 250
Processing Properties Metric English Comments
Processing Temperature 120 - 160 °C
248 - 320 °F
Sheet Forming