Material Notes:
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resistance. Designed to meet critical impulse and corona specifications.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
Water Absorption 0.15 %
0.15 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 39 - 45
39 - 45
ASTM D2583
Tensile Strength, Ultimate 124 MPa
18000 psi
ASTM D638
Flexural Strength 234 MPa
33900 psi
ASTM D790
Flexural Modulus 15.0 GPa
2180 ksi
ASTM D790
Compressive Strength 234 MPa
33900 psi
ASTM D695
Izod Impact, Notched 11.4 J/cm
21.4 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495