Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 1508 Polyester, Briquette, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1508 Polyester, Briquette, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is available in gray.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.940 g/cc
0.0340 lb/in³
ASTM D1895
Density 2.07 g/cc
0.0748 lb/in³
ASTM D792
Water Absorption 0.11 %
0.11 %
ASTM D570
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 67
67
ASTM D785
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 0.86 %
0.86 %
ASTM D638
Tensile Modulus 12.1 GPa
1750 ksi
ASTM D638
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Compressive Strength 139 MPa
20200 psi
ASTM D695
Poissons Ratio 0.283
0.283
ASTM D638
Shear Modulus 4.72 GPa
685 ksi
Calculated
Izod Impact, Notched 0.272 J/cm
0.510 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.255 J/cm²
1.21 ft-lb/in²
ASTM D256
Impact 172
172
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 40.0 - 130 °C
33.3 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 218 °C
424 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 233 °C
451 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.0117 %
0.0117 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+15 ohm-cm
1.40e+15 ohm-cm
ASTM D247
Dielectric Constant 5.0
5.0
ASTM D150
Dielectric Strength 10.6 kV/mm
269 kV/in
Step by Step; ASTM D149
12.6 kV/mm
320 kV/in
Short Time; ASTM D149
Dielectric Breakdown 22800 V
22800 V
ASTM D149
Dissipation Factor 0.0139
0.0139
ASTM D150
Arc Resistance 184 sec
184 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638