Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Impact Grade, Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particularly suited for mechanical parts with thin sections that require wheelabrating, staking or pulling of inserts.Data provided by Plaslok Corporation.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Water Absorption 1.0 %
1.0 %
ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
Compression; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 8.30 GPa
1200 ksi
ASTM D790
Compressive Yield Strength 221 MPa
32100 psi
ASTM D695
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
351 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Constant 4.2
4.2
1MHz; ASTM D150
6.8
6.8
60 Hz; ASTM D150
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Dissipation Factor 0.040
0.040
1 MHz; ASTM D150
0.090
0.090
60 Hz; ASTM D150