Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The ARC 5ES is kneaded by hand to mix the components, which are then simply applied to the surface to be repaired. The 5ES hardens in 5-7 minutes and cures to full strength in 30 minutes. Its putty like consistency and moisture insensitive chemistry resist washout when repairing leaks. Cures under water, bonds to wet surfaces, 100% solids, non-shrinking. Benefits:Once cured, seals 3 mm (1/8”) leaks up to seven atmospheres (100 psi).Putty like viscosity resist washout when sealing leaksBonds and cures under waterTough resin structure resists thermal mechanical shockLabor and down time are reduced due to ease of use and rapid curingConvenient packaging is easily carried in pocket or tool boxColor change verifies complete mixCures down to 4°C (40°F)Benchmark tested to be the best available technology for leak repairsARC 5ES is certified by NSF to NSF/ANSI Standard 61. Suggested Uses:Stop Leaks:PipesAir DuctsFiberglassConduitsRadiatorsValvesPumpsPoolsRepair:Cracked Battery CasingsLavatory FixturesCracked Tile & MarbleFasten or Adhere:SignsTemporary FixturesInformation provided by Chesterton
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Compressive Strength 27.6 MPa
4000 psi
ASTM D695
Adhesive Bond Strength 11.7 MPa
1700 psi
Unclean; ASTM D1002
15.2 MPa
2200 psi
SSPC SP3-Wet; ASTM D1002
29.0 MPa
4200 psi
SSPC SP3-Dry; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 54.0 °C
129 °F
Wet
121 °C
250 °F
Dry
Electrical Properties Metric English Comments
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 9.00 min
0.150 hour
Cure Time to 90% Shore D
4.98 min

@Temperature 32.0 °C
0.0830 hour

@Temperature 89.6 °F
Initial Set
15.0 min

@Temperature 16.0 °C
0.250 hour

@Temperature 60.8 °F
Initial Set
19.8 min

@Temperature 4.00 °C
0.330 hour

@Temperature 39.2 °F
Initial Set
30.0 min

@Temperature 32.0 °C
0.500 hour

@Temperature 89.6 °F
Full Chemical
45.0 min

@Temperature 25.0 °C
0.750 hour

@Temperature 77.0 °F
Full Chemical
60.0 min

@Temperature 16.0 °C
1.00 hour

@Temperature 60.8 °F
Full Chemical
75.0 min

@Temperature 4.00 °C
1.25 hour

@Temperature 39.2 °F
Full Chemical
100 min

@Temperature 25.0 °C
1.67 hour

@Temperature 77.0 °F
Initial Set