Polymer Property : Dielectric Strength = 3050 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 13.0 - 120 kV/mm
330 - 3050 kV/in
Average value: 25.5 kV/mm Grade Count:20
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Dielectric Strength 11.8 - 120 kV/mm
300 - 3050 kV/in
Average value: 34.3 kV/mm Grade Count:109
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Dielectric Strength 9.84 - 120 kV/mm
250 - 3050 kV/in
Average value: 31.2 kV/mm Grade Count:101
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Dielectric Strength 15.7 - 120 kV/mm
400 - 3050 kV/in
Average value: 23.4 kV/mm Grade Count:200
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Dielectric Strength 13.8 - 120 kV/mm
350 - 3050 kV/in
Average value: 50.9 kV/mm Grade Count:6
Overview of materials for Nylon 66, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri..
Copyright © lookpolymers.com All Rights Reserved