Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 08112 Polyester BMC, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 08112 Polyester BMC, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its combination of high heat resistance, good electrical properties and strength, it can be used in such applications as iron skirts and other small appliance housings, coil bobbins, and electric motor components such as brush holders. It is available in either bulk or extruded form and is currently available in natural. Other colors are available upon request. It is UL recognized under file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Density 2.03 g/cc
0.0733 lb/in³
ASTM D792
Water Absorption 0.093 %
0.093 %
ASTM D570
Linear Mold Shrinkage 0.00228 cm/cm
0.00228 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 52
52
ASTM D785
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Elongation at Break 0.39 %
0.39 %
ASTM D638
Tensile Modulus 16.6 GPa
2410 ksi
ASTM D638
Flexural Strength 89.0 MPa
12900 psi
ASTM D790
Flexural Modulus 14.0 GPa
2030 ksi
ASTM D790
Compressive Strength 125 MPa
18100 psi
ASTM D695
Izod Impact, Notched 2.37 J/cm
4.44 ft-lb/in
ASTM D256
Charpy Impact, Notched 2.31 J/cm²
11.0 ft-lb/in²
ASTM D256
Impact 810
810
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 228 °C
442 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 267 °C
513 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.00 %
0.00 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 9.90e+15 ohm-cm
9.90e+15 ohm-cm
ASTM D247
Dielectric Constant 4.9
4.9
ASTM D150
Dielectric Strength 9.70 kV/mm
246 kV/in
Step by Step; ASTM D149
11.8 kV/mm
300 kV/in
Short Time; ASTM D149
Dielectric Breakdown 23000 V
23000 V
1hr 120C; ASTM D149
Dissipation Factor 0.0096
0.0096
ASTM D150
Arc Resistance 188 sec
188 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638